Hastelloy C22 Flanges Supplier Maharashtra | Delta Superalloys LLP

Hastelloy C22 Flanges Supplier Maharashtra

Hastelloy C22 Flanges Supplier Maharashtra

If you are in Maharashtra and looking for a reliable Hastelloy C22 flanges supplier, Delta Superalloys LLP is your trusted partner. We supply high-quality Hastelloy C22 flanges to industrial hubs across Maharashtra — including Mumbai, Pune, Nashik, Aurangabad, Thane, Raigad, Nagpur, and more. Our Hastelloy C22 flanges are manufactured to the highest standards, offering exceptional corrosion resistance, mechanical strength, and reliability in the most demanding applications across chemical processing, oil & gas, pharmaceutical, and power generation industries.

Why Hastelloy C22 Flanges Are the Preferred Choice

Hastelloy C22 (UNS N06022) is one of the most versatile corrosion-resistant alloys available today. Flanges made from Hastelloy C22 offer superior strength, reliability, and resistance to aggressive environments compared to standard steel flanges. The alloy's exceptional properties make it the preferred choice for critical applications.

Key advantages of Hastelloy C22 flanges include:

  • Exceptional resistance to pitting, crevice corrosion, and stress corrosion cracking
  • Excellent performance in both oxidizing and reducing environments
  • High mechanical strength across a wide temperature range (-196°C to 1093°C)
  • Excellent resistance to localized corrosion
  • Reliable leak-proof connections in critical applications
  • Good fabricability and weldability

Our Range of Hastelloy C22 Flanges

We supply a comprehensive range of Hastelloy C22 flanges:

  • Weld Neck Flanges — Class 150 to 2500
  • Slip-On Flanges — Class 150 to 2500
  • Blind Flanges — Class 150 to 2500
  • Socket Weld Flanges — Class 150 to 2500
  • Threaded Flanges — Class 150 to 2500
  • Lap Joint Flanges — Class 150 to 2500
  • Orifice Flanges — Class 300 to 2500
  • Plate Flanges — Class 150 to 2500
  • Custom Flanges as per drawing

If your project requires custom sizes or specifications, we can manufacture flanges to meet your exact requirements.

Dimensions and Specifications

  • Standards: ASTM B564 / ASME SB564, ASTM B462 / ASME SB462
  • Flange Standards: ANSI/ASME B16.5, B16.47, API 6A, MSS-SP-44
  • Size Range: ½" NB to 24" NB (larger sizes available on request)
  • Class Range: 150, 300, 400, 600, 900, 1500, 2500
  • Condition: Solution annealed and pickled
  • Surface Finish: As per customer requirement

Technical Specifications

Material Hastelloy C22 (UNS N06022)
Standards ASTM B564 / ASME SB564, ASTM B462 / ASME SB462
Flange Standards ANSI/ASME B16.5, B16.47, API 6A
Size Range ½" NB to 24" NB
Class Range 150 to 2500
Condition Solution Annealed & Pickled
Surface Finish As per customer requirement

Quality Assurance and Documentation

Every consignment of Hastelloy C22 flanges we supply is accompanied by comprehensive documentation:

  • Mill Test Certificates (MTC) as per EN 10204 3.1
  • Chemical and mechanical test reports
  • Positive Material Identification (PMI) on request
  • Third-party inspection through Lloyd's, BV, TUV, or SGS
  • Full heat-to-finish traceability
  • Dimensional inspection and surface quality check
  • NACE MR0175 / MR0103 compliance where required

If your project requires specific approvals beyond what's listed here, mention it during your inquiry — in most cases, we can arrange it through our testing partners.

Industries We Serve Across Maharashtra

We supply Hastelloy C22 flanges to a wide range of industries across Maharashtra:

  • Chemical Processing: Reactor vessels, heat exchangers, and piping systems
  • Pharmaceutical Manufacturing: API reactors and high-purity equipment
  • Power Generation: Boiler components and turbine parts
  • Pulp and Paper: Bleaching lines and digesters
  • Oil and Gas: Offshore and onshore equipment
  • Pollution Control: Flue gas desulfurization systems
  • Aerospace & Defense: High-performance components

Why Choose Delta Superalloys LLP

With our base in Mumbai, we are strategically positioned to serve the entire state of Maharashtra efficiently. Here's why clients trust us:

  • ISO 9001:2015 certified operations
  • Genuine, verifiable mill certificates with every shipment
  • Ready stock of commonly used sizes
  • Expert technical support for grade selection
  • Competitive pricing and timely delivery
  • Two decades of experience in high-nickel alloy supply
  • Dedicated export packaging for international shipments
  • Custom manufacturing capabilities for special requirements

Packaging & Delivery

  • Export-quality wooden crates and pallets for safe transit
  • Standard delivery: 3-5 days (domestic - Maharashtra & India)
  • Export delivery: 7-15 days (international)
  • Full documentation with every shipment
  • Custom packaging solutions available on request

Request a Quote

For an accurate quote on Hastelloy C22 flanges, please send us your requirements — flange type, size, class, quantity, and any certification needs. We will respond with competitive pricing and delivery timelines. You can reach us through the contact form below, over WhatsApp, or by calling us directly.

📩 Request a Quote →
Serving Across Maharashtra

Mumbai • Pune • Nashik • Aurangabad • Thane • Raigad • Nagpur • and more

❓ Frequently Asked Questions

We supply a complete range including weld neck, slip-on, blind, socket weld, threaded, lap joint, orifice, and custom flanges as per customer drawings.
We manufacture as per ASTM B564 / ASME SB564, ASTM B462 / ASME SB462, ANSI/ASME B16.5, B16.47, and API 6A standards.
Yes. Positive Material Identification (PMI) testing is available on request to ensure material integrity before dispatch.
We provide Mill Test Certificates (MTC) as per EN 10204 3.1, chemical and mechanical test reports, and full traceability documentation. Third-party inspection can also be arranged.
Yes. We can manufacture custom flanges as per your drawings and specifications. Contact us with your requirements.
Yes. We export Hastelloy C22 flanges to international clients with complete documentation and packaging suited for overseas shipment.