Hastelloy C22 Round Bar Manufacturer Mumbai
When you need high-performance materials for aggressive chemical environments, Hastelloy C22 round bars are often the first choice. At Delta Superalloys LLP, we are a premier Hastelloy C22 round bar manufacturer in Mumbai, producing high-quality round bars that meet the most demanding industrial specifications. Our manufacturing facility in Mumbai allows us to serve clients across India and internationally with precision-engineered Hastelloy C22 round bars that deliver exceptional corrosion resistance and mechanical strength.
Why Hastelloy C22 Round Bars Are in High Demand
Hastelloy C22 (UNS N06022) is one of the most versatile corrosion-resistant alloys in the market. It was developed specifically to withstand a wide range of aggressive chemicals — including wet chlorine, hypochlorite, chlorine dioxide, sulphuric acid, and hydrochloric acid — environments where most stainless steels and even many nickel alloys would fail.
What makes C22 particularly valuable is its ability to perform in both oxidizing and reducing environments. This dual capability means fewer material changes in complex process streams, making it the preferred choice for chemical processing, pharmaceutical manufacturing, and pollution control equipment.
Key properties of Hastelloy C22 include:
- Exceptional resistance to pitting, crevice corrosion, and stress corrosion cracking
- Excellent resistance to localized corrosion
- Outstanding performance in both oxidizing and reducing environments
- High mechanical strength across a wide temperature range (-196°C to 1093°C)
- Good fabricability and weldability
Our Manufacturing Range
We manufacture Hastelloy C22 round bars in the following specifications:
- Standard: ASTM B574 / ASME SB574
- UNS Designation: N06022
- Diameter Range: 6mm to 300mm
- Length: Standard random lengths or cut-to-size
- Condition: Solution annealed and pickled
- Surface Finish: Black, machined, or bright
- Tolerance: As per ASTM standards
If your project requires sizes or finishes outside our standard range, we can manufacture custom sizes to meet your exact specifications.
Chemical Composition (Typical)
- Nickel (Ni): Balance (56.0% min)
- Chromium (Cr): 20.0 – 22.5%
- Molybdenum (Mo): 12.5 – 14.5%
- Iron (Fe): 2.0 – 6.0%
- Tungsten (W): 2.5 – 3.5%
- Cobalt (Co): 2.5% max
- Manganese (Mn): 0.5% max
- Silicon (Si): 0.08% max
- Carbon (C): 0.015% max
Technical Specifications
| Standard |
ASTM B574 / ASME SB574 |
| UNS Designation |
N06022 |
| Diameter Range |
6mm - 300mm |
| Length |
Random / Cut-to-size |
| Condition |
Solution Annealed & Pickled |
| Surface Finish |
Black, Machined, Bright |
| Tolerance |
As per ASTM standards |
Quality Assurance and Testing
Every batch of Hastelloy C22 round bars manufactured by Delta Superalloys LLP undergoes rigorous quality testing. Our quality assurance process includes:
- Mill Test Certificates (MTC) as per EN 10204 3.1
- Chemical composition analysis
- Mechanical property testing (tensile, hardness, impact)
- Positive Material Identification (PMI) on request
- Third-party inspection through Lloyd's, BV, TUV, or SGS
- Full heat-to-finish traceability
- Dimensional inspection and surface quality check
If your project requires specific approvals beyond what's listed here, mention it during your inquiry — in most cases, we can arrange it through our testing partners.
Industries We Serve
We manufacture Hastelloy C22 round bars for a wide range of industries across Mumbai and beyond:
- Chemical Processing: Reactor vessels, heat exchangers, and piping systems
- Pharmaceutical Manufacturing: API reactors and high-purity equipment
- Power Generation: Boiler components and turbine parts
- Pulp and Paper: Bleaching lines and digesters
- Oil and Gas: Offshore and onshore equipment
- Pollution Control: Flue gas desulfurization systems
- Aerospace & Defense: High-performance components
Why Choose Delta Superalloys LLP as Your Manufacturer
With our manufacturing facility in Mumbai, we offer several advantages to our clients:
- ISO 9001:2015 certified manufacturing operations
- In-house manufacturing capabilities for better quality control
- Genuine, verifiable mill certificates with every shipment
- Competitive pricing through efficient production processes
- Expert technical support for alloy selection and application advice
- Two decades of experience in high-nickel alloy manufacturing
- Quick turnaround times for urgent requirements
- Dedicated export packaging for international shipments
Packaging & Delivery
- Export-quality wooden crates and pallets for safe transit
- Standard delivery: 3-5 days (domestic - Mumbai & India)
- Export delivery: 7-15 days (international)
- Full documentation with every shipment
- Custom packaging solutions available on request
Request a Quote
For an accurate quote on Hastelloy C22 round bars, please send us your requirements — diameter, length, quantity, finish, and any certification needs. We will respond with competitive pricing and delivery timelines. You can reach us through the contact form below, over WhatsApp, or by calling us directly.