Hastelloy C22 Round Bars Manufacturer In Mumbai | Delta Super Alloys

Hastelloy C22 Round Bars

Hastelloy C22 Round Bars Supplier | Delta Super Alloys LLP

Hastelloy C22 Round Bars

Delta Super Alloys LLP offers premium-quality Hastelloy C22 Round Bars, developed to deliver exceptional corrosion resistance in the most demanding chemical environments. This nickel-chromium-molybdenum alloy is especially effective against localized corrosion mechanisms such as pitting and crevice attack.

Compared to conventional nickel alloys, Hastelloy C22 provides superior resistance in both oxidizing and reducing media, making it a preferred choice for critical components used in chemical processing equipment, marine systems, pharmaceutical plants, and oil & gas installations. Delta Super Alloys LLP supplies round bars in customized diameters, lengths, and surface finishes as per client requirements.

Key Features

  • Outstanding resistance to pitting, crevice corrosion, and cracking
  • High mechanical strength with excellent structural stability
  • Very good weldability and fabrication characteristics
  • Reliable performance in mixed acid and chloride environments
  • Enhanced corrosion resistance compared to Hastelloy C276
  • Supplied in custom sizes with full material traceability

Product Specifications

UNS No N06022
Standard Hastelloy C22 Round Bars
Round Bar Size 3mm dia to 1000mm dia
Square Bar Size 6mm dia to 800mm dia
Flat Bar Size 1.6mm to 2000mm
Hex Bar Size 2mm dia to 800mm dia
Angle Size 3mm x 20mm x 20mm to 20mm x 200mm x 200mm
Length 100mm to 6000mm
Forms Round, Square, Hex, Flat, Billet, Forging
Element Percentage (%)
Nickel (Ni) Balance
Chromium (Cr) 20.0 – 22.5
Molybdenum (Mo) 12.5 – 14.5
Iron (Fe) 2.0 – 6.0
Tungsten (W) 2.5 – 3.5
Cobalt (Co) ≤ 2.5
Carbon (C) ≤ 0.01
Manganese (Mn) ≤ 0.5
Silicon (Si) ≤ 0.08
Grade UNS Ni Cr Mo Fe W Co C Mn Si P Others
Hastelloy C22 N06022 Balance 20.0–22.5 12.5–14.5 2.0–6.0 2.5–3.5 ≤2.5 ≤0.01 ≤0.5 ≤0.08 ≤0.02 V ≤ 0.35
Tensile Strength ≥ 690 MPa
Yield Strength ≥ 310 MPa
Elongation ≥ 45%
Density 8.69 g/cm³
Melting Range 1325 – 1370°C

Chemical Processing

Hastelloy C22 Round Bars are extensively used in chemical processing industries for reactors, heat exchangers, columns, and piping systems handling aggressive acids and corrosive chemicals.

Oil & Gas

Ideal for oil & gas environments including sour gas wells, offshore platforms, and downhole equipment due to excellent resistance to sulfide stress cracking.

Marine

Suitable for marine and offshore applications where exposure to seawater, salt spray, and high chloride environments is common.

Power Generation

Widely used in flue gas desulfurization units, heat exchangers, and power plant components requiring corrosion and oxidation resistance.

Pharmaceutical

Used in pharmaceutical manufacturing equipment where high purity, corrosion resistance, and contamination-free processing are critical.

Need Hastelloy C22 Round Bars?

Contact us today for premium quality Hastelloy C22 Round Bars tailored to your requirements.