When it comes to handling some of the toughest chemical environments in the industry, Hastelloy C22 Round Barsis a name engineers turn to again and again. At Delta Super Alloys LLP, we manufacture and supply this nickel-chromium-molybdenum alloy in premium quality, built specifically to stand up to aggressive corrosion, especially the kind that attacks in isolated spots like pits and crevices rather than spreading evenly across a surface.
What sets Hastelloy C22 Round Bars apart from many other nickel-based alloys is its versatility. It performs reliably whether it's exposed to oxidizing conditions or reducing ones, which is exactly why it's so widely trusted across chemical plants, marine equipment, pharmaceutical facilities, and oil & gas operations. At Delta Super Alloys LLP, every bar we supply can be tailored in diameter, length, and finish to match your project needs, and each batch comes with complete traceability so you always know exactly what you're getting.
| UNS No | N06022 |
|---|---|
| Standard | Hastelloy C22 Round Bars |
| Round Bar Size | 3mm dia to 1000mm dia |
| Square Bar Size | 6mm dia to 800mm dia |
| Flat Bar Size | 1.6mm to 2000mm |
| Hex Bar Size | 2mm dia to 800mm dia |
| Angle Size | 3mm x 20mm x 20mm to 20mm x 200mm x 200mm |
| Length | 100mm to 6000mm |
| Forms | Round, Square, Hex, Flat, Billet, Forging |
| Element | Percentage (%) |
|---|---|
| Nickel (Ni) | Balance |
| Chromium (Cr) | 20.0 – 22.5 |
| Molybdenum (Mo) | 12.5 – 14.5 |
| Iron (Fe) | 2.0 – 6.0 |
| Tungsten (W) | 2.5 – 3.5 |
| Cobalt (Co) | ≤ 2.5 |
| Carbon (C) | ≤ 0.01 |
| Manganese (Mn) | ≤ 0.5 |
| Silicon (Si) | ≤ 0.08 |
| Grade | UNS | Ni | Cr | Mo | Fe | W | Co | C | Mn | Si | P | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Hastelloy C22 | N06022 | Balance | 20.0–22.5 | 12.5–14.5 | 2.0–6.0 | 2.5–3.5 | ≤2.5 | ≤0.01 | ≤0.5 | ≤0.08 | ≤0.02 | V ≤ 0.35 |
| Tensile Strength | ≥ 690 MPa |
|---|---|
| Yield Strength | ≥ 310 MPa |
| Elongation | ≥ 45% |
| Density | 8.69 g/cm³ |
| Melting Range | 1325 – 1370°C |
Hastelloy C22 Round Bars are extensively used in chemical processing industries for reactors, heat exchangers, columns, and piping systems handling aggressive acids and corrosive chemicals.
Ideal for oil & gas environments including sour gas wells, offshore platforms, and downhole equipment due to excellent resistance to sulfide stress cracking.
Suitable for marine and offshore applications where exposure to seawater, salt spray, and high chloride environments is common.
Widely used in flue gas desulfurization units, heat exchangers, and power plant components requiring corrosion and oxidation resistance.
Used in pharmaceutical manufacturing equipment where high purity, corrosion resistance, and contamination-free processing are critical.