Hastelloy C22 Wires

Hastelloy C22 Wires Supplier | Delta Super Alloys LLP

Hastelloy C22 Wires

When a project calls for corrosion resistance without compromising on dimensional accuracy, Hastelloy C22 Wires consistently deliver. Delta Super Alloys LLP supplies these high-purity wires for applications where mechanical reliability matters just as much as chemical resistance. Made from a nickel-chromium-molybdenum alloy, this grade holds up well against localized corrosion even in some of the harshest chemical environments around.

When a project calls for corrosion resistance without compromising on dimensional accuracy, Hastelloy C22 Wires consistently deliver. Delta Super Alloys LLP supplies these high-purity wires for applications where mechanical reliability matters just as much as chemical resistance. Made from a nickel-chromium-molybdenum alloy, this grade holds up well against localized corrosion even in some of the harshest chemical environments around.

Key Features

  • Strong resistance to pitting, crevice corrosion, and chemical attack
  • High tensile strength combined with good flexibility for easier handling
  • Stable mechanical properties even at elevated temperatures
  • Offered as filler wire, coil wire, or straight cut lengths
  • Consistent diameter and a clean, high-quality surface finish
  • Long service life with dependable, repeatable performance

Product Specifications

UNS No N06022
Standard Hastelloy C22 Wires
Diameter 0.1mm to 100mm
Length 100mm to 6000mm (Custom Cut Length)
Form Filler Wire, Coil Wire, Straight Wire, etc.
Grade Werkstoff UNS Ni Cr Co Mo Fe Cu Nb Al Ti C S Si Mn Others
Hastelloy C22 2.4602 N06022 Remainder 20.0 – 22.5 2.5 Min 12.5 – 14.5 2.0 – 6.0 - - - - 0.015 Max 0.02 Max 0.08 Max 0.50 Max W 2.5–3.5 / V 0.35 Min / P 0.02 Max
Tensile Strength (Rm) 690 MPa
Yield Strength (Rp0.2) 310 MPa
Elongation (A5) 45%
Density 8.69 g/cm³

Welding Applications

Used as filler wires for welding corrosion-resistant alloys.

Chemical Processing

Equipment exposed to aggressive chemicals and acidic environments.

Oil & Gas

Sour gas processing, offshore platforms, and harsh environments.

Marine & Pharmaceutical

High-purity and corrosion-resistant wire applications.

Need Hastelloy C22 Wires?

Contact us today for premium-quality Hastelloy C22 wires manufactured to your exact specifications.

Request a Quote