Hastelloy C276 Round Bars Manufacturer In Mumbai | Delta Super Alloys

Hastelloy C276 Round Bars

Hastelloy C276 Round Bars Supplier | Delta Super Alloys LLP

Hastelloy C276 Round Bars

Few alloys handle aggressive corrosion as well as Hastelloy C276 Round Bars. Delta Super Alloys LLP is a trusted manufacturer, exporter, and supplier of this high-performance nickel-molybdenum-chromium alloy, known for standing strong in environments that would eat through lesser materials. These round bars offer outstanding protection against pitting, crevice corrosion, and stress corrosion cracking, making them a go-to choice wherever chemical attack is a serious concern.

We produce our Hastelloy C276 Round Bars in line with international quality standards, and they're widely used across chemical processing, pollution control, oil & gas, marine, and power generation industries. Since project requirements rarely look the same twice, Delta Super Alloys LLP also offers customized sizes and finishes to match your exact specifications.

Key Features:

  • Excellent resistance to pitting, crevice, and stress corrosion cracking
  • High strength and durability, even in extreme operating environments
  • Strong fabricability and weldability for smoother project execution
  • Dependable performance across chemical, oil & gas, and marine applications
  • Custom sizes and specifications available to match client needs

Product Specifications

UNS No N10276
Standard Hastelloy C276 Round Bars
Round Bar Size 3mm dia to 1000mm dia
Square Bar Size 6mm dia to 800mm dia
Flat Bar Size 1.6mm to 2000mm thickness
Finish Black, Bright, Polished
Form Round Bars, Hex Bars, Square Bars
Hex Bar Size 2mm dia to 800mm dia
Length 100mm to 6000mm (Custom Cut Length)
Angle Size 3mm x 20mm x 20mm to 20mm x 200mm x 200mm
Thickness 1.6mm to 100mm
GRADE Werkstoff UNS Ni Cr Co Mo Fe Cu Nb Al Ti C S Si Mn Others
Hastelloy C276 2.4819 N10276 57.00 114.5 - 16.5 2.50 15.0 - 17.0 4.0 - 7.0 - - - - 0.01 0.01 0.08 1.00 W - 3 - 4.5 / V - 0.35 / P - 0.025
Important Notes:

All values are in percentage (%). "-" indicates element is not intentionally added or present only in trace amounts. Nickel (Ni) is the balance element.

💪
Tensile Strength
690 MPa
(minimum)
📏
Yield Strength
283 MPa
(0.2% offset)
↔️
Elongation
40%
⚖️
Density
8.89 g/cm³
Property Value Test Method
Hardness (Rockwell B) ≤ 100 HRB ASTM E18
Modulus of Elasticity 205 GPa ASTM E111
Thermal Conductivity 10.1 W/m·K @ 100°C
Melting Range 1325 - 1370°C -
🏭

Chemical Processing

Reactors, vessels, heat exchangers, and piping systems handling corrosive chemicals.

🛢️

Oil & Gas

Downhole components, valves, pumps, and fittings in sour gas environments.

🌊

Marine Engineering

Components exposed to seawater and marine atmospheres with high chloride content.

⚡

Power Generation

Flue gas desulfurization systems, scrubbers, and pollution control equipment.

🧪

Pharmaceutical

Equipment for aggressive pharmaceutical processes requiring high purity.

🏗️

Pulp & Paper

Digesters, bleach plants, and other equipment in corrosive pulp processing.

Need Hastelloy C276 Round Bars?