Delta Super Alloys LLP offers premium-grade Hastelloy C276 Sheets, Plates & Coils developed to perform reliably in extremely corrosive and high-pressure environments. This alloy combines excellent corrosion resistance with superior structural stability, even under severe operating conditions.
Our Hastelloy C276 flat products are precision processed to ensure uniform thickness, smooth surface finish, and consistent mechanical properties. These materials are extensively used for fabrication of process equipment, heat exchangers, storage vessels, and piping systems in chemical, oil & gas, pharmaceutical, and power generation industries.
| UNS No | N10276 |
|---|---|
| Standard | Hastelloy C276 Sheets, Plates & Coils |
| Thickness | 0.1mm thk to 100mm thk |
| Width | 100mm to 2000mm |
| Length | 100mm to 6000mm (Custom Cut Length) |
| Forms | Coils, Shims, Plates, Sheets, Strips, Flats |
| Finish | Hot Rolled plate (HR), Cold Rolled Plate (CR) 2B, 2D, etc. |
| Hardness | Soft, Hard, Half Hard, Quarter hard, Spring hard etc. |
| Grade | Werkstoff | UNS | Ni | Cr | Co | Mo | Fe | Cu | Nb | Al | Ti | C | S | Si | Mn | Others |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Hastelloy C276 | 2.4819 | N10276 | 57.00 | 14.5 - 16.5 | 2.50 | 15.0 - 17.0 | 4.0 - 7.0 | - | - | - | - | 0.01 | 0.01 | 0.08 | 1.00 | W 3–4.5 / V 0.35 / P 0.025 |
| Tensile Strength (Rm) | 690 MPa |
|---|---|
| Yield Strength (Rp0.2) | 285 MPa |
| Elongation (A5) | 40% |
| Density | 8.89 g/cm³ |
Used in reactors, heat exchangers, and chemical handling equipment.
Ideal for offshore platforms and sour gas applications.
Flue gas desulfurization systems and heat exchangers.
Clean and corrosion-resistant processing equipment.
Contact us today for high-quality Hastelloy C276 sheets, plates, and coils with fast delivery and competitive pricing.
Request a QuoteCall us: +91 9653155322